PETG First Layer on an Ender 3: The Order to Fix It

An Ender 3 fails PETG at the first layer for reasons that barely exist on a Bambu: the bed is glass or a thin flexible sheet, the gantry is not rigid, and the machine is usually in a cold room. Work through those before touching the slicer.
The bed surface decides everything
PETG on bare glass bonds to the point of taking chips out of the glass. That is not a tuning problem, it is a release problem, and the standard answers are:
| Bed | PETG behaviour | What to do |
|---|---|---|
| Bare glass | bonds permanently | glue stick as release, every time |
| Textured PEI sheet | good grip | clean, no glue |
| Smooth PEI | strong grip | thin glue layer on large parts |
If you are still on the stock glass sheet, add a glue stick before you change any setting. Removing a welded PETG part from glass is how plates get ruined.
The bed mesh is worse than you think
An Ender 3 bed typically bows in the middle or dips at the corners, often by more than the first layer height. On PLA at 0.2 mm you might get away with it. On PETG, which is less forgiving, a bed that varies by 0.1 mm will produce a first layer that is squished on one side and floating on the other.
Run a manual mesh with a sheet of paper at five points, or a probe if you have one, and look at the numbers. If the spread is larger than about a quarter of your first-layer height, fix the mechanical cause first: loose eccentric nuts, a warped carriage, or a bed that needs shimming.
Cold room, cold part
PETG shrinks as it cools, and an Ender in an unheated room creates a large temperature gradient across the first layer. This is why the same profile works in summer and fails in winter. Two options: enclose the printer, or raise the bed temperature by 5 °C and slow the first layer down.
Speed on a bed-slinger
The bed moves, and PETG is heavy when it is hot. Printing the first layer fast on an Ender means the part is thrown around before it has stuck. Halve your PLA first-layer speed, and reduce acceleration for the first layer if your firmware allows it.
The order that works
- Release agent on glass. Before anything else.
- Clean the surface. Warm water and dish soap, air dry.
- Check the mesh numbers. Fix physical problems, not the slicer.
- Bed to 75–80 °C. Higher than PLA, and higher again in a cold room.
- First-layer speed at roughly half. And first-layer fan off.
- Flow calibration last. Only after the above hold.
One trap specific to the Ender 3
The stock PTFE-lined hotend starts to degrade around 240 °C, and PETG wants the upper end of that range. If you have been printing PETG hot for a while, a partly degraded liner shows up as intermittent under-extrusion that no first-layer adjustment fixes. If the flow looks fine cold and starved hot, look at the liner before the settings.
FAQ
Can I print PETG on the stock Ender 3 glass bed? Yes, but use a glue stick as a release agent. Without it parts weld to the glass and take chips with them.
Why does PETG stick in the middle and not at the corners? That pattern is a bed mesh problem, not a temperature problem. Measure the bed and fix the mechanical cause.
What bed temperature for PETG on an Ender 3? Around 75 °C, and 80 °C in a cold room. Below 70 the corners lift on larger parts.
Should the part cooling fan be on for the first layer? No. Keep it off for layer one so the PETG bonds, then bring it in gradually.
Why does my PETG print fine on small parts and fail on large ones? Shrinkage. The larger the footprint, the more the first layer is pulled as it cools. Slower first layer and a warmer bed both help.